SS 310S Stainless Steel 2B Finish Sheets
Surface treatment: 2b, Ba, No.1, No.4, Hl, 8K, etc.
Thickness: 0.1mm-300mm or as required
Width: 3mm-2000mm or as required
Delivery time: 7-15 days
Transportation packaging: waterproof paper and steel belt packaging.
Capacity: 8000 tons/year
310S2B Finish Cold Rolled 310S Stainless Steel Sheets supplier
As a leading supplier of stainless steel sheets, GNEE offers premium 310S 2B finish stainless steel sheets strictly manufactured in accordance with ASTM A240 standards. The surface is cold rolled, annealed, and pickled to ensure a smooth, scale-free finish with surface roughness Ra <= 1.6μm. Available in thicknesses from 0.3mm to 6.0mm with tight thickness tolerance within ±0.05mm, we support widths from 1000mm to 3000mm, custom length cutting, and coil supply. Laser cutting, polishing, and other value-added processing services are also available upon request.
All sheets come with EN 10204 3.2 certificates, third-party inspection reports, free samples, technical support, and fast delivery, covering everything from sample testing to full-scale production.
310S stainless steel sheet with 2B finish offers high dimensional precision, with a thickness tolerance controlled within ±0.05mm, making it suitable for applications that require exact sizing. The 2B surface is smooth and clean, produced through cold rolling, annealing, and pickling processes. The pickling effectively removes surface oxides, making it an ideal base for further finishing treatments such as polishing. It is well-suited for corrosive environments in industries such as chemical processing and food manufacturing.
310S 2B surface finish stainless steel sheet features a hardness of <=187HB. During cold bending and stamping, the stress is evenly distributed (with a recommended bending radius >= 2 times the sheet thickness), ensuring excellent formability. Its cost is lower than BA or mirror-polished finishes, offering a cost-effective solution without compromising performance-ideal for large-scale industrial applications.

| SS 310S (UNS S31008, EN 1.4845) | |
| ASTM A240 / A240M | |
| 2B (Smooth, bright, slightly reflective surface) | |
| 0.3 mm – 6.0 mm | |
| 1000 mm – 1500 mm (custom available) | |
| 2000 mm – 6000 mm (or customized) | |
| ±0.05 mm | |
| >= 515 MPa | |
| >= 205 MPa | |
| Elongation (50mm gauge) | >= 35% |
| <= 187 HB | |
| 1150℃ | |
| Max Short-Term Use Temp | 1200℃ |
310S stainless steel 2B finish sheets price
we supply high-quality SS 310S stainless steel 2B finish sheets with full material traceability and mill test certifications. Our products are available in stock sizes or custom dimensions, with fast delivery and competitive prices.


buy 310S stainless steel cold rolled sheet




Népszerű tags: ss 310s stainless steel 2b finish sheets, China ss 310s stainless steel 2b finish sheets manufacturers, suppliers, factory, rozsdamentes acéllemez, rozsdamentes acéllemez logisztikában, rozsdamentes acéllemez kutatásban, rozsdamentes acéllemez -kiskereskedő, rozsdamentes acéllemez vastagsága, rozsdamentes acéllemez nagykereskedő